Objective: To evaluate bond strength achieved by 3 commercially available self etching primers & to determine whether Xeno V & Clearfil Protect Bond self etching primers are suitable for orthodontic use. Method: The products tested were 1. Transbond Plus Self Etching Primer,3M 2. Xeno V, Dentsply,3. Clearfil Protect Bond, Japan.60 freshly extracted human maxillary 1st premolars were randomly divided into 3 groups of 20 teeth each. Group 1 (Transbond Plus Self Etching Primer & Transbond XT) group 2 (Xeno V and Transbond XT) group 3 (Clearfil Protect Bond & Transbond XT). Self etching primers were applied according to manufacturer?s recommendations & metal brackets in all groups were bonded with Transbond XT adhesive. Brackets were cured for 20 sec with halogen curing lamp & stored for 24 hrs in distilled water. Brackets were debonded in shear on a universal testing machine. Results: One-way ANOVA showed a statistically significant difference. Group 3 had the highest shear bond strength. Conclusions: Acceptable bond strength was achieved by all the 3 groups tested. . Xeno V & Clearfil Protect Bond self-etching primers had sufficient shear bond strength to withstand normal orthodontic force.

Medios de comunicación Libros     Paperback Book   (Libro con tapa blanda y lomo encolado)
Publicado 25 de abril de 2013
ISBN13 9783659374791
Editores LAP LAMBERT Academic Publishing
Páginas 88
Dimensiones 150 × 5 × 225 mm   ·   149 g
Lengua Alemán