How Do Flowing Conditions Affect Copper / Aisi 304 Galvanic Corrosion?: Electrochemical Study on Heavy Lithium Bromide Brines - José García-antón - Libros - LAP LAMBERT Academic Publishing - 9783844314656 - 1 de marzo de 2011
En caso de que portada y título no coincidan, el título será el correcto

How Do Flowing Conditions Affect Copper / Aisi 304 Galvanic Corrosion?: Electrochemical Study on Heavy Lithium Bromide Brines

Precio
Mex$ 851
sin IVA

Pedido desde almacén remoto

Entrega prevista 16 - 26 de nov.
Los regalos de Navidad se podrán canjear hasta el 31 de enero
Recibe notificaciones sobre nuevos lanzamientos de José García-antón
Añadir a tu lista de deseos de iMusic

Aún no valorado

Absorption cooling is a suitable alternative to refrigeration compression systems which use refrigerants that are responsible for the ozone layer depletion and the climate change. Despite the fact that lithium bromide is the most commonly used absorbent in absorption systems, it contains bromides, which cause corrosion problems. Additionally, the fluid flow can enhance these problems. Copper and stainless steels are widely used in the construction of absorption systems. This book provides a comprehensive study of the influence of Reynolds number (including a hydraulic circuit design)on the galvanic corrosion of the copper/AISI 304 stainless steel pair in heavy lithium bromide brines using electrochemical techniques. Results can be useful for those who develop their research in the electrochemical field, where there is a lack of studies about corrosion taking into consideration flowing conditions. Moreover, the results could be of interest for engineers who want to know the real corrosion behaviour in pipelines and to understand the novel zero resistance ammeter technique, which allows monitoring corrosion without disturbing the system under investigation and in continuous-time.

Medios de comunicación Libros     Paperback Book   (Libro con tapa blanda y lomo encolado)
Publicado 1 de marzo de 2011
ISBN13 9783844314656
Editores LAP LAMBERT Academic Publishing
Páginas 76
Dimensiones 226 × 5 × 150 mm   ·   131 g
Lengua Alemán